This paper details the influence of the welding parameters of submerged arc welding in the hardness of welded joint of S235JR construction steel. The planned experiment work is conducted in the semiautomatic submerged arc welding machine and the contribution of each factor has been considering, such as: (intensity, voltage, trolley welding speed, diameter of the wire, wire speed, cooling speed of the welded joint, OK Flux 1071, chemical properties of material and wire). The results of the present investigation indicate that the welding voltage, current intensity and environment of cooling of the welded joint are the most significant factors that controls the hardness of bead. Optimal results were obtained by using the tension of 37 V, intensity of 350 A at a trolley speed of 6.0 mm/s and wire diameter 2.4 mm process, and how it helps to optimize the number of test cases that need to be done.
Keywords:
S235 Steel, Submerged Arc Welding, Welding Parameters, Weld bead, Hardness.
Proceedings Editor
Edmond Hajrizi
ISBN
978-9951-550-95-6
Location
UBT Lipjan, Kosovo
Start Date
28-10-2023 8:00 AM
End Date
29-10-2023 6:00 PM
DOI
10.33107/ubt-ic.2023.87
Recommended Citation
Smaili, Fidan and Ibishi, Hajredin, "Optimizing Welding Parameters of Submerged Arc Welding based on Hardness in S235JR Construction Steel" (2023). UBT International Conference. 4.
https://knowledgecenter.ubt-uni.net/conference/IC/mech/4
Optimizing Welding Parameters of Submerged Arc Welding based on Hardness in S235JR Construction Steel
UBT Lipjan, Kosovo
This paper details the influence of the welding parameters of submerged arc welding in the hardness of welded joint of S235JR construction steel. The planned experiment work is conducted in the semiautomatic submerged arc welding machine and the contribution of each factor has been considering, such as: (intensity, voltage, trolley welding speed, diameter of the wire, wire speed, cooling speed of the welded joint, OK Flux 1071, chemical properties of material and wire). The results of the present investigation indicate that the welding voltage, current intensity and environment of cooling of the welded joint are the most significant factors that controls the hardness of bead. Optimal results were obtained by using the tension of 37 V, intensity of 350 A at a trolley speed of 6.0 mm/s and wire diameter 2.4 mm process, and how it helps to optimize the number of test cases that need to be done.